Ecometalclay produces the highest quality metal clays

FYI Silver Clay

Drying temperature max 120C.

Firing in the kiln 30-90minutes at a temperature 840-890C

Shrinkage approx. 20%


FYI Sterling 960
One Phase Firing

Drying temperature max. 120C

Firing in the kiln 60-90 minutes at a temperature 870C

Shrinkage approx. 18%

FYI Bronze Clay

Drying temperature max 120C.

Two phase firing in the kiln:

1 binder burnout – 350C, 5 minutes

2 firing activated charcoal for in 1-3 hours at a temperature 790C -840C

Shrinkage approx. 10%


FYI Bronze Clay
One Phase Firing

Drying temperature max 100C

One phase firing 830C in activated charcoal for 2-3 hours.

Shrinkage approx. 10%

FYI Copper Clay

Drying temperature max 120C.

Two phase firing in the kiln:

1 binder burnout – 350C, 5 minutes

2 firing activated charcoal for in 1-3 hours at a temperature 910C - 960C

Shrinkage approx. 10%


FYI Copper Clay
One Phase Firing

Drying temperature max 100C

One phase firing 960C in activated charcoal for 2-3 hours.

Shrinkage approx. 10%